Product description
Name
|
Aluminum brazing flux |
Model
|
W-208F |
Components
|
Fluoride and active agent |
Physical Property
|
White liquid |
Melting Temperature
|
550-570℃ |
Soldering Temperature
|
580~620℃ |
Scope of Application
|
Suitable for hardware, electric heating and aluminum radiator industries together with aluminum brazing flux brazing aluminum and aluminum alloy |
Soldering Method
|
Frequency torch soldering |
Pre-soldering Preparation
|
Evenly apply on workpieces after sprinkling or soaking |
Soldering Property
|
Remove fluoride effectively, improve brazing flux’s wettability on base materials, enhance permeability of brazing flux and form protective film on workpieces without cleaning |
Executive Standard
|
JB/T6045-1992 |
Packing Method
|
20kg/barrel |
Cautions
|
Tighten the cap after use and keep it in a dry and cool place |
Wufu WeChat
Huizhou China Wonderful Industrial Technology Co., Ltd
ADD:Huicheng District,Huizhou City, Guangdong Province
ADD:+86-752-2893501 +86-752-2200396
WEB:www.cnwufu.com
E-MAIL:sales@cnwufu.com
COPYRIGHT © 2020 Huizhou China Wonderful Industrial Technology Co., Ltd ALL RIGHTS RESERVED 粤ICP备11048504号 Powered by www.300.cn